CNS standard heat resistant steel bar steel grade and chemical composition
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.35 | 0.45 | ||
Si | 1.80 | 2.50 | ||
Mn | - | 0.60 | ||
P | - | 0.030 | ||
S | - | 0.030 | ||
Cr | 10.00 | 12.00 | ||
Ni | - | 0.60 | ||
Mo | 0.70 | 1.30 | ||
N | - | - |
CNS standard heat resistant steel bar steel grade and chemical composition
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
415 (≥) | 993 (≥) | 34 | 24 | 34 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 143 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
558 (≥) | 527 (≥) | 23 | 24 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 411 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
982 | 872 | 765 |
We can customize the production of SUH3 grade, contact us for the best solution.