CNS standard heat resistant steel bar steel grade and chemical composition
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.75 | 0.85 | ||
Si | 1.75 | 2.25 | ||
Mn | 0.20 | 0.60 | ||
P | - | 0.030 | ||
S | - | 0.030 | ||
Cr | 19.00 | 20.50 | ||
Ni | 1.15 | 1.65 | ||
Mo | - | - | ||
N | - | - |
CNS standard heat resistant steel bar steel grade and chemical composition
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
624 (≥) | 963 (≥) | 41 | 21 | 33 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 122 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
173 (≥) | 746 (≥) | 22 | 24 | 43 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 431 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
922 | 681 | 487 |
We can customize the production of SUH4 grade, contact us for the best solution.
–sales@specificsteel.com