Nickel Alloy, Corrosion and Heat-Resistant, Sheet, Strip, and Plate 57Ni - 19.5Cr - 13.5Co - 4.2Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted, Annealed
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.07 | ||
Si | - | 0.10 | ||
Mn | - | 0.10 | ||
Cr | - | 19.75 | ||
Ni | - | remaining | ||
Mo | - | 4.45 | ||
Co | - | 14.00 | ||
W | - | - | ||
Al | - | 1.40 | ||
Cu | - | - | ||
Ti | - | 3.00 | ||
Fe | - | 0.75 | ||
B | - | 0.005 | ||
Zr | - | 0.04 |
Nickel Alloy, Corrosion and Heat-Resistant, Sheet, Strip, and Plate 57Ni - 19.5Cr - 13.5Co - 4.2Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted, Annealed
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
956 (≥) | 881 (≥) | 22 | 34 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 342 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
279 (≥) | 962 (≥) | 33 | 11 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 221 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
867 | 744 | 575 |
We can customize the production of Waspaloy grade, contact us for the best solution.