Steel FE-PM1901 (X12CrNi13) - 600 MPa <= Rm <= 800 MPa - Bars - De <= 70 mm
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.08 | 0.15 | ||
Si | - | 1.00 | ||
Mn | - | 1.50 | ||
P | - | 0.040 | ||
S | 0.15 | 0.35 | ||
Cr | 12.0 | 13.0 | ||
Ni | - | 0.60 |
Steel FE-PM1901 (X12CrNi13) - 600 MPa <= Rm <= 800 MPa - Bars - De <= 70 mm
Stainless steels - Technical delivery conditions for drawn wire
Stainless steels - Part 1: List of stainless steels
Ferritic stainless steel
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
847 (≥) | 867 (≥) | 21 | 22 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 412 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
386 (≥) | 245 (≥) | 13 | 14 | 43 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 312 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
356 | 543 | 726 |
We can customize the production of X12Cr13 grade, contact us for the best solution.