Armatures, building fittings, cutlery
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.08 | ||
Si | - | 1.00 | ||
Mn | - | 1.00 | ||
P | - | 0.040 | ||
S | - | 0.015 | ||
Cr | 12.0 | 14.0 | ||
Al | 0.10 | 0.30 |
Stainless steels - Technical delivery conditions for drawn wire
Ferritic stainless steel
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
128 (≥) | 137 (≥) | 44 | 12 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 213 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
947 (≥) | 547 (≥) | 23 | 24 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 344 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
255 | 381 | 345 |
We can customize the production of X6CrAI13 grade, contact us for the best solution.