Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.10 | 0.15 | ||
Si | - | 0.60 | ||
Mn | - | 0.60 | ||
P | - | 0.030 | ||
S | - | 0.025 | ||
Cr | 12.00 | 14.00 | ||
Ni | - | 0.60 | ||
Mo | 1.00 | 1.60 | ||
Ti | 2.60 | 3.20 | ||
Al | - | 0.12 | ||
B | - | 0.010 |
Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
859 (≥) | 731 (≥) | 23 | 31 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 114 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
912 (≥) | 777 (≥) | 22 | 22 | 14 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 334 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
717 | 436 | 238 |