A 276 317 Stainless Steels to A 276 (2010)

A 276 317 - Specification & Application

  • A 276 (2010) - Stainless Steel Bars and Shapes

Stainless Steel Bars and Shapes

Chemical composition(wt.%) of A 276 317 grade: to A 276 (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.03
Cr 18.00 20.00
Ni 11.00 15.00
Mo 3.00 4.00
N - 0.10

A 276 317 - Detail

Stainless Steel Bars and Shapes

Mechanical properties of grade A 276 317 A 276 (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
169 (≥) 484 (≥) 31 21 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 422

Physical properties of grade A 276 317 A 276 (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
338 (≥) 618 (≥) 41 31 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 344
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
815 575 854

Equivalent Products

We can customize the production of A 276 317 grade, contact us for the best solution.
sales@specificsteel.com