Chemical composition(wt.%) of A 276 S21904 grade: to A 276 (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.04
Si - 1.00
Mn 8.00 10.0
P - 0.06
S - 0.03
Cr 19.0 21.5
Ni 5.50 7.50
N 0.15 0.40

A 276 S21904 - Detail

A 276 S21904

Mechanical properties of grade A 276 S21904 A 276 (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
843 (≥) 592 (≥) 23 31 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 441

Physical properties of grade A 276 S21904 A 276 (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
734 (≥) 886 (≥) 13 31 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 423
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
623 567 269