Steel, Sheet, Strip, and Plate 1.05Cr - 0.55Ni - 1.0Mo - 0.12V (0.45 - 0.50C) Consumable Electrode Vacuum Melted
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.47 | ||
Si | - | 0.22 | ||
Mn | - | 0.75 | ||
P | - | - | ||
S | - | - | ||
Ni | - | 0.55 | ||
Cr | - | 1.05 | ||
Al | - | - | ||
Cu | - | - | ||
Ti | - | - | ||
Fe | - | remaining | ||
Mo | - | 1.00 | ||
Co | - | - | ||
V | - | 0.10 |
Steel, Sheet, Strip, and Plate 1.05Cr - 0.55Ni - 1.0Mo - 0.12V (0.45 - 0.50C) Consumable Electrode Vacuum Melted
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
594 (≥) | 164 (≥) | 34 | 34 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 332 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
743 (≥) | 953 (≥) | 31 | 12 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 433 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
625 | 682 | 684 |
We can customize the production of D6AC grade, contact us for the best solution.