Stellite alloy
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 1.30 | ||
Si | - | 1.20 | ||
Mn | - | - | ||
Cr | - | 31.00 | ||
Ni | - | 8.00 | ||
Mo | - | 8.00 | ||
Co | remaining | - | ||
W | - | 18.00 | ||
Fe | - | - |
Stellite alloy
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
282 (≥) | 842 (≥) | 34 | 23 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 231 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
296 (≥) | 395 (≥) | 44 | 42 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 323 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
445 | 546 | 239 |
We can customize the production of Stellite 2006 grade, contact us for the best solution.
–sales@specificsteel.com