Stainless steels - Part 3: Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.43 | 0.50 | ||
Si | - | 1.00 | ||
Mn | - | 1.00 | ||
P | - | 0.04 | ||
S | - | 0.015 | ||
Cr | 12.50 | 14.50 | ||
Ni | - | - | ||
Mo | - | - |
Stainless steels - Part 3: Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
235 (≥) | 668 (≥) | 41 | 43 | 21 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 431 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
577 (≥) | 389 (≥) | 23 | 14 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 233 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
667 | 581 | 949 |
We can customize the production of X46Cr13 grade, contact us for the best solution.