Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.08 | ||
Mn | - | 2.00 | ||
Si | - | 1.00 | ||
P | - | 0.045 | ||
S | - | 0.03 | ||
Cr | 17.00 | 19.00 | ||
Ni | 9.00 | 12.00 | ||
N | - | 0.10 |
Stainless Steel Spring Wire
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
173 (≥) | 693 (≥) | 14 | 24 | 14 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 322 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
879 (≥) | 186 (≥) | 24 | 43 | 21 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 412 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
155 | 676 | 718 |