Heat resisting steels and nickel alloys
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.03 | 0.10 | ||
Si | - | 0.50 | ||
Mn | - | 0.50 | ||
P | - | 0.020 | ||
S | - | 0.015 | ||
Cr | 20.00 | 23.00 | ||
Ni | 58.00 | - | ||
Al | - | 0.30 | ||
Ti | - | 0.40 | ||
Fe | - | 5.00 | ||
Cu | - | 0.50 | ||
Co | - | 1.00 | ||
Nb+Ta | 3.15 | 4.15 |
Heat resisting steels and nickel alloys
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
855 (≥) | 916 (≥) | 41 | 23 | 33 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 223 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
857 (≥) | 175 (≥) | 31 | 14 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 123 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
921 | 455 | 926 |
We can customize the production of NiCr22Mo9Nb grade, contact us for the best solution.
–sales@specificsteel.com