SUS 304 J3 Stainless Steels to G 4309 (1999)

SUS 304 J3 - Specification & Application

  • G 4309 (1999) - Stainless steel wires

Stainless steel wires

Chemical composition(wt.%) of SUS 304 J3 grade: to G 4309 (1999)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.03
Cr 17.00 19.00
Ni 8.00 10.50
Mo - -
N - -
Cu 1.00 3.00

SUS 304 J3 - Detail

Stainless steel wires

Mechanical properties of grade SUS 304 J3 G 4309 (1999)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
221 (≥) 972 (≥) 43 44 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 221

Physical properties of grade SUS 304 J3 G 4309 (1999)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
567 (≥) 913 (≥) 13 32 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 433
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
855 877 193

Equivalent Products

We can customize the production of SUS 304 J3 grade, contact us for the best solution.