X15CrNiSi20-12 Stainless Steels to ISO 15510 (2010)

X15CrNiSi20-12 - Specification & Application

  • ISO 15510 (2010) - Stainless steels -- Chemical composition
  • ISO 4955 (2005) - Heat-resistant steels

Heat-resistant steels

Chemical composition(wt.%) of X15CrNiSi20-12 grade: to ISO 15510 (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.20
Si 1.50 2.50
Mn - 2.00
P - 0.045
S - 0.030
Cr 19.00 21.00
Ni 11.00 13.00

X15CrNiSi20-12 - Detail

Heat-resistant steels

Mechanical properties of grade X15CrNiSi20-12 ISO 15510 (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
871 (≥) 818 (≥) 43 21 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 422

Physical properties of grade X15CrNiSi20-12 ISO 15510 (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
214 (≥) 365 (≥) 43 14 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 312
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
898 746 185