Specification for Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.16 | 0.24 | ||
Si | 3.20 | 4.00 | ||
Mn | - | 2.00 | ||
P | - | 0.03 | ||
S | - | 0.03 | ||
Cr | 17.0 | 19.5 | ||
Ni | 13.5 | 16.0 | ||
Al | 0.80 | 1.50 |
Specification for Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
845 (≥) | 876 (≥) | 14 | 24 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 313 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
982 (≥) | 742 (≥) | 43 | 23 | 31 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 423 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
574 | 274 | 799 |
We can customize the production of SA-213 S30615 grade, contact us for the best solution.