Chemical composition(wt.%) of SA-276 S28200 grade: to SA-276

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Mn 17.00 19.00
Si - 1.00
P - 0.045
S - 0.03
Cr 17.50 19.50
Ni - -
Mo 0.50 1.50
N 0.40 0.60
Cu 0.50 1.50

SA-276 S28200 - Detail

Specification for Stainless Steel Bars and Shapes

Mechanical properties of grade SA-276 S28200 SA-276

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
457 (≥) 677 (≥) 13 13 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 444

Physical properties of grade SA-276 S28200 SA-276

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
875 (≥) 769 (≥) 14 21 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 131
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
213 818 648

Equivalent Products

We can customize the production of SA-276 S28200 grade, contact us for the best solution.