Stainless steel for boiler and heat exchanger tubes
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.08 | ||
Si | 3.00 | 5.00 | ||
Mn | - | 2.00 | ||
P | - | 0.045 | ||
S | - | 0.030 | ||
Cr | 15.00 | 20.00 | ||
Ni | 11.50 | 15.00 | ||
Mo | - | - | ||
N | - | - |
Stainless steel for boiler and heat exchanger tubes
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
525 (≥) | 424 (≥) | 43 | 14 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 424 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
578 (≥) | 473 (≥) | 24 | 42 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 113 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
377 | 816 | 694 |
We can customize the production of STSXM15J1TB grade, contact us for the best solution.