Classification and designation for superalloys and high temperature intermetallic materials
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.08 | ||
Cr | 12.0 | 16.0 | ||
Ni | 35.0 | 40.0 | ||
W | 5.00 | 6.50 | ||
Al | 1.40 | 2.20 | ||
Ti | 2.40 | 3.20 | ||
Si | - | 0.60 | ||
Mn | - | 0.50 | ||
P | - | 0.015 | ||
S | - | 0.015 | ||
B | - | 0.02 | ||
Ce | - | 0.02 |
GH2130
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
611 (≥) | 467 (≥) | 23 | 23 | 31 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 212 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
825 (≥) | 474 (≥) | 24 | 24 | 41 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 111 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
427 | 345 | 745 |
We can customize the production of GH2130 grade, contact us for the best solution.
–sales@specificsteel.com