Stellite 2006 Tool Die Steels

Stellite 2006 - Specification & Application

Stellite alloy

Chemical composition(wt.%) of Stellite 2006 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 1.30
Si - 1.20
Mn - -
Cr - 31.00
Ni - 8.00
Mo - 8.00
Co remaining -
W - 18.00
Fe - -

Stellite 2006 - Detail

Stellite alloy

Mechanical properties of grade Stellite 2006

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
179 (≥) 477 (≥) 33 13 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 421

Physical properties of grade Stellite 2006

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
869 (≥) 296 (≥) 14 44 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 241
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
451 276 482

Equivalent Grade

Equivalent Products

We can customize the production of Stellite 2006 grade, contact us for the best solution.