Stellite alloy
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 2.30 | ||
Si | - | 1.00 | ||
Mn | - | 1.00 | ||
Cr | - | 31.00 | ||
Ni | - | 3.00 | ||
Mo | - | - | ||
Co | remaining | - | ||
W | - | 12.50 | ||
Fe | - | 3.00 | ||
B | - | 1.00 |
Stellite alloy
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
964 (≥) | 583 (≥) | 11 | 14 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 221 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
617 (≥) | 195 (≥) | 34 | 13 | 14 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 313 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
373 | 661 | 741 |
We can customize the production of Stellite 3PM grade, contact us for the best solution.