8Cr17 Stainless Steels to GB/T 1220 (1992)

8Cr17 - Specification & Application

  • GB/T 1220 (1992) - Stainless steel bars
  • GB/T 4356 (2002) - Stainless steel wire rods

Stainless steel bars

Chemical composition(wt.%) of 8Cr17 grade: to GB/T 1220 (1992)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.75 0.95
Si - 1.00
Mn - 1.00
P - 0.035
S - 0.030
Ni - 0.60
Cr 16.00 18.00
Mo - 0.75

8Cr17 - Detail

Mechanical properties of grade 8Cr17 GB/T 1220 (1992)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
829 (≥) 883 (≥) 12 41 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 122

Physical properties of grade 8Cr17 GB/T 1220 (1992)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
851 (≥) 434 (≥) 14 33 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 323
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
891 936 638

Equivalent Products

We can customize the production of 8Cr17 grade, contact us for the best solution.
sales@specificsteel.com