Nickel-base superalloy
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.05 | 0.10 | ||
Cr | 16.5 | 19.5 | ||
Mo | 2.5 | 3.5 | ||
Ni | - | Remainder | ||
Co | 13.5 | 16.5 | ||
W | 1.0 | 2.0 | ||
Al | 2.0 | 3.0 | ||
Ti | 4.5 | 5.5 | ||
B | 0.01 | 0.03 | ||
Fe | - | 1.0 | ||
Zr | - | 0.05 |
GH4710
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
949 (≥) | 973 (≥) | 42 | 12 | 41 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 131 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
239 (≥) | 391 (≥) | 42 | 31 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 133 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
595 | 571 | 388 |
We can customize the production of GH4710 grade, contact us for the best solution.