X12Cr13 Stainless Steels to NF EN 10088-1

X12Cr13 - Specification & Application

  • NF EN 10088-1 - Stainless steels - Part 1: List of stainless steels
  • NF EN 10088-2 - Stainless steels - Part 2: Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for general purposes
  • NF EN 10088-3 - Stainless steels - Part 3: Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes
  • NF EN 10088-4 - Stainless steels - Part 4: Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for construction purposes
  • NF EN 10088-5 - Stainless steels - Part 5: Technical delivery conditions for bars, rods, wire, sections and bright products of corrosion resisting steels for construction purposes
  • NF EN 10250-4 - Open die steel forgings for general engineering purposes - Part 4: Stainless steels
  • NF EN 10263-5 - Steel rod, bars and steel wire for cold heading and cold extrusion - Part 5: Technical delivery conditions for stainless steels
  • NF EN 10272 - Stainless steel bars for pressure purposes
  • NF EN 10297-2 (2005) - Seamless circular steel tubes for mechanical and general engineering purposes - Technical delivery conditions - Part 2: Stainless steel

Seamless circular steel tubes for mechanical and general engineering purposes - Technical delivery conditions - Part 2: Stainless steel

Chemical composition(wt.%) of X12Cr13 grade: to NF EN 10088-1

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.08 0.15
Si - 1.00
Mn - 1.00
P - 0.040
S - 0.015
Cr 11.50 13.50
Mo - -
Ni - 0.75

X12Cr13 - Detail

Seamless circular steel tubes for mechanical and general engineering purposes - Technical delivery conditions - Part 2: Stainless steel

Mechanical properties of grade X12Cr13 NF EN 10088-1

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
642 (≥) 129 (≥) 22 24 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 344

Physical properties of grade X12Cr13 NF EN 10088-1

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
599 (≥) 369 (≥) 23 11 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 441
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
879 823 991

Equivalent Products