Based on 0cr19ni9 plus N, strength increase and the plastic is not down. Reduce the thickness of the material. As a structure with strength components
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.08 | ||
Si | - | 1.00 | ||
Mn | - | 2.00 | ||
P | - | 0.035 | ||
S | - | 0.030 | ||
Ni | 7.00 | 10.50 | ||
Cr | 18.00 | 20.00 | ||
N | 0.10 | 0.25 |
Stainless and heat resisting steels
GB 13296 (2007) Seamless stainless steel tubes for boiler and heat exchanger
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
366 (≥) | 744 (≥) | 22 | 11 | 43 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 241 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
613 (≥) | 847 (≥) | 24 | 24 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 134 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
972 | 314 | 675 |
We can customize the production of 0Cr19Ni9N grade, contact us for the best solution.