1.3541 Stainless Steels to DIN 17230 (1980)

1.3541 - Specification & Application

  • DIN 17230 (1980) - Ball and Roller Bearing Steels; Technical Conditions of Delivery

Corrosion-resistant high-temperature steel

Chemical composition(wt.%) of 1.3541 grade: to DIN 17230 (1980)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.35 0.44
Si - 0.6
Mn - 0.6
Ni - 0.6
S - 0.025
P - 0.03
Cr 12 14

1.3541 - Detail

Corrosion-resistant high-temperature steel

Mechanical properties of grade 1.3541 DIN 17230 (1980)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
857 (≥) 232 (≥) 42 33 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 341

Physical properties of grade 1.3541 DIN 17230 (1980)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
887 (≥) 766 (≥) 21 32 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 231
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
348 112 998
We can customize the production of 1.3541 grade, contact us for the best solution.