Welded Austenitic Steel Boiler, Superheater, Heat-Exchanger, and Condenser Tubes
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.02 | ||
Mn | - | 1.00 | ||
Si | - | 0.80 | ||
P | - | 0.03 | ||
S | - | 0.01 | ||
Cr | 19.50 | 20.50 | ||
Ni | 17.50 | 18.50 | ||
Mo | 6.00 | 6.50 | ||
Cu | 0.50 | 1.00 | ||
N | 0.18 | 0.22 |
Welded Austenitic Steel Boiler, Superheater, Heat-Exchanger, and Condenser Tubes
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
811 (≥) | 221 (≥) | 32 | 43 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 334 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
637 (≥) | 411 (≥) | 11 | 34 | 41 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 422 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
368 | 476 | 891 |
We can customize the production of A 249 S31254 grade, contact us for the best solution.
–sales@specificsteel.com