Nickel-base superalloy
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.08 | ||
Cr | 14.0 | 17.0 | ||
Ni | - | Remainder | ||
Co | - | 1.0 | ||
Al | 0.4 | 1.0 | ||
Nb+Ta | 0.7 | 1.2 | ||
Ti | 2.25 | 2.75 | ||
Fe | 5.0 | 7.0 |
GH4145
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
365 (≥) | 951 (≥) | 13 | 21 | 42 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 123 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
684 (≥) | 635 (≥) | 32 | 21 | 14 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 324 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
824 | 431 | 949 |
We can customize the production of GH4145 grade, contact us for the best solution.
–sales@specificsteel.com