A 493 S44625 Stainless Steels to A 493 (2009)

A 493 S44625 - Specification & Application

  • A 493 (2009) - Stainless Steel Wire and Wire Rods for Cold Heading and Cold Forging

Stainless Steel Wire and Wire Rods for Cold Heading and Cold Forging

Chemical composition(wt.%) of A 493 S44625 grade: to A 493 (2009)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.01
Mn - 0.40
Si - 0.40
P - 0.02
S - 0.02
Cr 25.00 27.00
Ni - 0.50
Mo 0.75 1.50
N - 0.015
Cu 0.20 -

A 493 S44625 - Detail

Stainless Steel Wire and Wire Rods for Cold Heading and Cold Forging

Mechanical properties of grade A 493 S44625 A 493 (2009)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
251 (≥) 361 (≥) 11 44 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 334

Physical properties of grade A 493 S44625 A 493 (2009)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
785 (≥) 326 (≥) 13 33 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 123
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
675 513 184

Equivalent Products

We can customize the production of A 493 S44625 grade, contact us for the best solution.