Austenitic stainless steel. Grade 00Cr17Ni14Mo2 was replaced by new designation 022Cr17Ni12Mo2 according to GB/T 20878 (2007)
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.030 | ||
Si | - | 1.00 | ||
Mn | - | 2.00 | ||
P | - | 0.035 | ||
S | - | 0.030 | ||
Ni | 12.00 | 15.00 | ||
Cr | 16.00 | 18.00 | ||
Mo | 2.00 | 3.00 |
Stainless and heat resisting steels
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
284 (≥) | 959 (≥) | 11 | 14 | 21 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 442 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
959 (≥) | 578 (≥) | 11 | 34 | 21 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 414 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
192 | 823 | 386 |
We can customize the production of 00Cr17Ni14Mo2 grade, contact us for the best solution.