Alloy Bars, Forgings, and Rings, Corrosion and Heat Resistant 54Ni - 17.5Cr - 16.5Co - 4.0Mo - 2.9Ti - 2.9Al - 0.006B Solution, Stabilization, and Precipitation Heat Treated Consumable Electrode or Vacuum Induction Melted
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.05 | 0.10 | ||
Si | - | 0.10 | ||
Mn | - | 0.10 | ||
Cr | - | 19.00 | ||
Ni | - | remaining | ||
Mo | - | 4.00 | ||
Co | - | 19.00 | ||
W | - | - | ||
Al | - | 3.00 | ||
Cu | - | - | ||
Ti | - | 3.00 | ||
Fe | - | - | ||
Zr | - | 0.06 | ||
B | - | 0.005 |
Alloy Bars, Forgings, and Rings, Corrosion and Heat Resistant 54Ni - 17.5Cr - 16.5Co - 4.0Mo - 2.9Ti - 2.9Al - 0.006B Solution, Stabilization, and Precipitation Heat Treated Consumable Electrode or Vacuum Induction Melted
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
773 (≥) | 157 (≥) | 31 | 31 | 14 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 332 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
695 (≥) | 693 (≥) | 32 | 12 | 34 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 221 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
756 | 535 | 846 |
We can customize the production of Udimet 500 grade, contact us for the best solution.