Nimonic 80A / NiCr20TiAl(2.4952) / UNS N07080/ BS 3HR1

Nimonic 80A / NiCr20TiAl(2.4952) / UNS N07080/ BS 3HR1

Nimonic 80A / NiCr20TiAl(2.4952) / UNS N07080/ BS 3HR1

  • Delivery status: Forged 、Solutioned 、
  • Surface: Polished 、
  • Standard: ASTM
  • Shape: Round,Flat,Square,Hexagon,Plate,Sheet etc

Product Details

GE spec NB 00146, Ideally released to GE spec NB 00146 or  to ASTM B637 or WK 2.4952 or BS 3HR1, VIM+ESR, Hot Forging,Polishing,

Grade

2.4952

Nimonic 80A

C

0.04~0.10

0.10

Si

1.00

1.00

Mn

1.00

1.00

P

0.020

S

0.015

0.015

Ni

65.00

Balance

Cr

18.00~21.00

18.00~21.00

Ti

1.80~2.70

1.80~2.70

Al

1.00~1.80

1.00~1.80

Co

1.00

2.00

Fe

1.50

3.00

Cu

0.20

0.20

B

0.008

0.008

Zr

0.15

Pb

0.0025


Supply Ability

Supply Ability: 5000 Ton/Tons per Month Stainless Steel Bar

Related Grade

Packaging & Delivery

We can customize the production of Nimonic 80A / NiCr20TiAl(2.4952) / UNS N07080/ BS 3HR1, contact us for the best solution.