Classification and designation for superalloys and high temperature intermetallic materials
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.08 | ||
Cr | 13.5 | 16.5 | ||
Mo | 1.00 | 1.50 | ||
Ni | 24.0 | 27.0 | ||
Al | - | 0.40 | ||
Ti | 1.75 | 2.30 | ||
Si | - | 1.00 | ||
Mn | - | 2.00 | ||
P | - | 0.030 | ||
S | - | 0.020 | ||
B | 0.001 | 0.010 | ||
V | 0.10 | 0.50 |
GH2132
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
563 (≥) | 486 (≥) | 34 | 32 | 41 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 134 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
548 (≥) | 464 (≥) | 24 | 11 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 211 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
722 | 992 | 377 |
We can customize the production of GH2132 grade, contact us for the best solution.