NCF625 Stainless Steels to D 3531 (2007)

NCF625 - Specification & Application

  • D 3531 (2007) - Corrosion - resisting and heat - resisting superalloy bars
  • D 3532 (2002) - Corrosion - resisting and heat - resisting superalloy plates and sheets

Corrosion - resisting and heat - resisting superalloy plates and sheets

Chemical composition(wt.%) of NCF625 grade: to D 3531 (2007)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.10
Si - 0.50
Mn - 0.50
P - 0.015
S - 0.015
Cr 20.00 23.00
Ni 58.00 -
Cu - -
Al - 0.40
Ti - 0.40
Fe - 5.00
Nb+Ta 3.15 4.15
Mo 8.00 10.00

NCF625 - Detail

Corrosion - resisting and heat - resisting superalloy plates and sheets

Mechanical properties of grade NCF625 D 3531 (2007)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
112 (≥) 255 (≥) 34 43 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 424

Physical properties of grade NCF625 D 3531 (2007)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
823 (≥) 146 (≥) 21 12 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 131
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
574 942 515

Equivalent Products

We can customize the production of NCF625 grade, contact us for the best solution.