S44025 Stainless Steels

S44025 - Specification & Application

S44025

Chemical composition(wt.%) of S44025 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.95 1.1
Si - 1.00
Mn - 1.00
P - 0.025
S - 0.025
Cr 16.0 18.0
Ni - 0.75
Mo 0.40 0.65

S44025 - Detail

S44025

Mechanical properties of grade S44025

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
718 (≥) 527 (≥) 21 21 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 424

Physical properties of grade S44025

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
416 (≥) 771 (≥) 13 13 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 434
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
118 151 656