Heat Resisting and Highly Heat Resisting Materials for Bolts and Nuts; Quality Specifications
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.16 | 0.22 | ||
Si | 0.10 | 0.50 | ||
Mn | 0.30 | 0.80 | ||
P | - | 0.035 | ||
S | - | 0.035 | ||
Cr | 10.0 | 11.5 | ||
Mo | 0.50 | 1.00 | ||
Ni | 0.30 | 0.80 | ||
V | 0.10 | 0.30 | ||
Nb | 0.15 | 0.50 | ||
N | 0.05 | 0.19 |
Heat Resisting and Highly Heat Resisting Materials for Bolts and Nuts; Quality Specifications
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
457 (≥) | 829 (≥) | 34 | 24 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 333 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
492 (≥) | 971 (≥) | 33 | 12 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 331 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
772 | 479 | 467 |
We can customize the production of X19CrMoVNbN11-1 grade, contact us for the best solution.