Nichrome V Stainless Steels to SAE J 470 (1976)

Nichrome V - Specification & Application

  • SAE J 470 (1976) - Wrought nickel and nickel-related alloys

Wrought nickel and nickel-related alloys

Chemical composition(wt.%) of Nichrome V grade: to SAE J 470 (1976)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si 0.75 1.60
Mn - 2.50
Cr 19.00 21.00
Ni - remaining
Mo - -
Co - -
W - -
Al - -
Cu - -
Ti - -
Fe - 1.00
S - 0.01

Nichrome V - Detail

Wrought nickel and nickel-related alloys

Mechanical properties of grade Nichrome V SAE J 470 (1976)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
758 (≥) 855 (≥) 33 34 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 414

Physical properties of grade Nichrome V SAE J 470 (1976)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
731 (≥) 127 (≥) 22 34 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 123
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
918 755 392

Equivalent Products

We can customize the production of Nichrome V grade, contact us for the best solution.