STS41603 Stainless Steels to D 7202 (2004)

STS41603 - Specification & Application

  • D 7202 (2004) - Free - machining stainless steel wire and wire rods

Free - machining stainless steel wire and wire rods

Chemical composition(wt.%) of STS41603 grade: to D 7202 (2004)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si - 1.00
Mn - 1.25
P - 0.060
S - 0.15
Cr 12.00 14.00
Ni - 0.60
Mo - 0.60
N - -

STS41603 - Detail

Free - machining stainless steel wire and wire rods

Mechanical properties of grade STS41603 D 7202 (2004)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
235 (≥) 367 (≥) 11 44 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 332

Physical properties of grade STS41603 D 7202 (2004)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
756 (≥) 228 (≥) 11 44 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 114
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
189 878 553