17-4 PH Stainless Steels to MIL-C-24111B

17-4 PH - Specification & Application

  • MIL-C-24111B - Chromium-nickel alloy steel bars, rods and forgings, corrosion resistant

Chromium-nickel alloy steel bars, rods and forgings, corrosion resistant

Chemical composition(wt.%) of 17-4 PH grade: to MIL-C-24111B

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.04
Si - 0.60
Mn - 0.28
Cr - 16.0
Ni - 4.25
Cu - 3.3
Fe - remaining
Nb - 0.27

17-4 PH - Detail

Chromium-nickel alloy steel bars, rods and forgings, corrosion resistant

Mechanical properties of grade 17-4 PH MIL-C-24111B

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
693 (≥) 882 (≥) 12 22 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 233

Physical properties of grade 17-4 PH MIL-C-24111B

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
823 (≥) 454 (≥) 41 21 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 244
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
498 843 723

Equivalent Grade

Equivalent Products

We can customize the production of 17-4 PH grade, contact us for the best solution.
sales@specificsteel.com