17-7 PH Stainless Steels

17-7 PH - Specification & Application

High temperature alloys and other special alloys

Chemical composition(wt.%) of 17-7 PH grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.07 -
Si 0.30 -
Mn 0.50 -
Cr 17.0 -
Ni 7.1 -
Al 1.17 -
Fe remaining -

17-7 PH - Detail

High temperature alloys and other special alloys

Mechanical properties of grade 17-7 PH

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
766 (≥) 699 (≥) 33 24 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 342

Physical properties of grade 17-7 PH

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
967 (≥) 122 (≥) 24 33 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 322
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
521 851 838

Equivalent Grade

Equivalent Products

We can customize the production of 17-7 PH grade, contact us for the best solution.