5642 Type 2 Stainless Steels to SAE AMS 5642K (2006)

5642 Type 2 - Specification & Application

  • SAE AMS 5642K (2006) - Steel, Corrosion and Heat-Resistant, Bars, Wire, and Forgings 18Cr - 10.5Ni - 0.60Cb Free-Machining, Solution Heat Treated

Steel, Corrosion and Heat-Resistant, Bars, Wire, and Forgings 18Cr - 10.5Ni - 0.60Cb Free-Machining, Solution Heat Treated

Chemical composition(wt.%) of 5642 Type 2 grade: to SAE AMS 5642K (2006)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.22
Si - 0.40
Mn - 0.75
P - -
S - -
Ni - 0.75
Cr - 12.50
Al - -
Cu - -
Ti - -
Fe - remaining
N - -
Mo - 1.00
W - 1.00
V - 0.22

5642 Type 2 - Detail

Steel, Corrosion and Heat-Resistant, Bars, Wire, and Forgings 18Cr - 10.5Ni - 0.60Cb Free-Machining, Solution Heat Treated

Mechanical properties of grade 5642 Type 2 SAE AMS 5642K (2006)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
413 (≥) 329 (≥) 13 32 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 344

Physical properties of grade 5642 Type 2 SAE AMS 5642K (2006)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
473 (≥) 688 (≥) 44 32 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 434
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
433 414 156
We can customize the production of 5642 Type 2 grade, contact us for the best solution.