A 815 WPS41008 Stainless Steels to A 815/A 815M (2010)

A 815 WPS41008 - Specification & Application

  • A 815/A 815M (2010) - Wrought Ferritic, Ferritic/Austenitic, and Martensitic Stainless Steel Piping Fittings

Wrought Ferritic, Ferritic/Austenitic, and Martensitic Stainless Steel Piping Fittings

Chemical composition(wt.%) of A 815 WPS41008 grade: to A 815/A 815M (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Mn - 1.00
Si - 1.00
P - 0.04
S - 0.03
Cr 11.50 13.50
Ni - 0.60
Mo - -

A 815 WPS41008 - Detail

Wrought Ferritic, Ferritic/Austenitic, and Martensitic Stainless Steel Piping Fittings

Mechanical properties of grade A 815 WPS41008 A 815/A 815M (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
272 (≥) 614 (≥) 12 13 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 433

Physical properties of grade A 815 WPS41008 A 815/A 815M (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
347 (≥) 213 (≥) 23 12 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 442
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
652 916 326