F 899 Type XM-13 Stainless Steels to F 899 (2012)

F 899 Type XM-13 - Specification & Application

  • F 899 (2012) - Standard Specification for Wrought Stainless Steels for Surgical Instruments

Standard Specification for Wrought Stainless Steels for Surgical Instruments

Chemical composition(wt.%) of F 899 Type XM-13 grade: to F 899 (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.05
Mn - 0.20
Si - 1.00
P - 0.01
S - 0.008
Cr 12.25 13.00
Ni 7.50 8.50
Mo 2.00 2.50
Al 0.90 1.35
N - 0.01

F 899 Type XM-13 - Detail

Standard Specification for Wrought Stainless Steels for Surgical Instruments

Mechanical properties of grade F 899 Type XM-13 F 899 (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
557 (≥) 987 (≥) 23 33 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 343

Physical properties of grade F 899 Type XM-13 F 899 (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
991 (≥) 479 (≥) 44 11 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 223
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
449 355 666