06X18H11 Stainless Steels

06X18H11 - Specification & Application

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(wt.%) of 06X18H11 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.06
Si - 0.80
Mn - 2.00
P - 0.035
S - 0.020
Cr 17.00 19.00
Ni 10.00 12.00
Mo - 0.30
W - 0.20
Ti - 0.20

06X18H11 - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 06X18H11

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
577 (≥) 784 (≥) 31 34 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 424

Physical properties of grade 06X18H11

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
415 (≥) 344 (≥) 12 14 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 231
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
193 813 944

Equivalent Grade

Equivalent Products

We can customize the production of 06X18H11 grade, contact us for the best solution.