Non-alloy quality steel
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.18 | 0.23 | ||
Si | - | 0.4 | ||
Mn | 0.3 | 0.9 | ||
Ni | - | 0.3 | ||
P | - | 0.025 | ||
S | - | 0.015 | ||
Cr | - | 0.3 | ||
Ti | - | 0.03 | ||
N | 0.03 | 0.07 | ||
Nb | - | 0.010 | ||
Al | 0.0015 | 0.05 | ||
V | - | 0.02 | ||
other | - | Cr+Cu+Mo+Ni < 0.7 |
1.0460
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
582 (≥) | 499 (≥) | 11 | 41 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 423 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
763 (≥) | 311 (≥) | 14 | 14 | 34 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 311 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
952 | 439 | 739 |
We can customize the production of 1.0460 grade, contact us for the best solution.
–sales@specificsteel.com