1.1830 Tool Die Steels

1.1830 - Specification & Application

High carbon steel

Chemical composition(wt.%) of 1.1830 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.80 0.90
Si 0.25 0.40
Mn 0.50 0.70
P - 0.025
S - 0.020

1.1830 - Detail

High carbon steel

Mechanical properties of grade 1.1830

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
233 (≥) 442 (≥) 14 33 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 343

Physical properties of grade 1.1830

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
276 (≥) 323 (≥) 11 11 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 424
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
942 185 975