1.2083 Tool Die Steels

1.2083 - Specification & Application

Tools high alloyed Cr steel

Chemical composition(wt.%) of 1.2083 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.38 0.45
Si - 1.00
Mn - 1.00
P - 0.030
S - 0.030
Cr 12.00 13.50
Mo - -
V - -

1.2083 - Detail

Tools high alloyed Cr steel

Mechanical properties of grade 1.2083

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
998 (≥) 597 (≥) 14 33 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 221

Physical properties of grade 1.2083

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
889 (≥) 831 (≥) 24 14 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 143
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
724 894 465

Equivalent Grade

Equivalent Products

We can customize the production of 1.2083 grade, contact us for the best solution.