1.2085 Tool Die Steels

1.2085 - Specification & Application

Free-cutting high alloyed Cr steel

Chemical composition(wt.%) of 1.2085 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.28 0.38
Si - 1.00
Mn - 1.00
P - 0.030
S 0.05 0.10
Cr 15.00 17.00
Mo - -
V - -
Ni - 1.00

1.2085 - Detail

Free-cutting high alloyed Cr steel

Mechanical properties of grade 1.2085

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
176 (≥) 853 (≥) 24 34 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 233

Physical properties of grade 1.2085

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
596 (≥) 226 (≥) 32 33 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 323
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
819 629 434

Equivalent Grade

Equivalent Products

We can customize the production of 1.2085 grade, contact us for the best solution.