1.2363 Tool Die Steels

1.2363 - Specification & Application

Alloyed CrMoV steel

Chemical composition(wt.%) of 1.2363 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.90 1.05
Si 0.20 0.40
Mn 0.40 0.70
P - 0.035
S - 0.035
Cr 4.80 5.50
Mo 0.90 1.20
V 0.10 0.30

1.2363 - Detail

Alloyed CrMoV steel

Mechanical properties of grade 1.2363

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
161 (≥) 695 (≥) 13 14 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 433

Physical properties of grade 1.2363

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
792 (≥) 481 (≥) 44 14 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 434
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
346 282 621

Equivalent Grade

Equivalent Products

We can customize the production of 1.2363 grade, contact us for the best solution.