1.7361 Structural Steel to DIN17211 (1987)

1.7361 - Specification & Application

  • DIN17211 (1987) - Nitriding steel

Nitriding steel

Chemical composition(wt.%) of 1.7361 grade: to DIN17211 (1987)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.28 0.35
Si - 0.40
Mn 0.40 0.70
P - 0.035
S - 0.035
Cr 2.80 3.30
Mo 0.30 0.50
Ni - 0.60

1.7361 - Detail

Nitriding steel

Mechanical properties of grade 1.7361 DIN17211 (1987)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
647 (≥) 348 (≥) 21 23 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 314

Physical properties of grade 1.7361 DIN17211 (1987)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
256 (≥) 325 (≥) 44 14 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 421
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
517 644 357

Equivalent Grade

Equivalent Products

We can customize the production of 1.7361 grade, contact us for the best solution.